LSAW steel pipe are manufactured of metal in-house produced and smelted in the electric furnace, treated with synthetic slags and cast by continuous casters. The applied steel making process ensures the achievement of chemically pure steel with reference to sulphur and phosphor contents providing high tensile, ductility and corrosion resistance properties of pipes to be operated at low temperatures in various corrosion media.
Rolling using a press piercing mill and continuous mill equipped with a fixed mandrel allows strict measurement tolerances to be obtained and ensures a lack of pipe body and surface defects.
In order to achieve high tensile and ductility steel as well as its required structure, providing a high corrosion resistance in various corrosion media, pipes are heat treated in a computerized walking beam furnace. 70% of oil line pipes are subject to heat treatment.
Pipes are inspected for internal and external flows by automatic non-distructive testing of ultrasonic and electromagnetic inspection. Pipe ends inspection after beveling is done by magnetic-fluoroscopic flaw detection.
While manufacturing seamless line pipes ensures testing of corrosion-resistance properties through hydrogen included cracking method under NACE MR 02-84 and sulphide stress corrosion cracking method under NACE MR 01-77.
The purpose of api 5l gr.b seamless pipe is suitable for useing in conveying gas, water, and oil in both oil and natural gas industries.
Standard | Grade | C | Mn | P | S |
API 5L | B | ≤0.28 | ≤1.20 | ≤0.030 | ≤0.030 |
Standard | Grade | yield strength(mpa) | tensile strength(mpa) | elongation(%) |
API 5L | B | 241 | 414 | 21-27 |
API 5l X52 is oil pipeline standard.
The API SPEC 5L covers seamless line pipe and welded line pipe.
Usage: for oil, natural gas industry, oxygen, water, oil pipeline; may also be used in the construction of engineering infrastructure, the Linyuan road beautification, drainage channels, the plant steel hook building, high-voltage power tower.
Standard | C(%) | Ti(%) | Mn(%) | P(%) | S(%) |
API 5L X52 | 0.28 | 0.04 | 1.40 | 0.03 | 0.03 |
API 5L X52 mechanical protert Standard Yield Strength(Mpa) Tensile Strength(Mpa) API 5L X52 359-531 455-758
|